What is the actual chemical for regular solvent? I have hunch that PEG 400 is the ideal chemical to use, but I'm lacking refrences. Anyone informed enough to confirm?
http://en.wikipedia.org/wiki/Polyethylene_glycol
Wik. says that PEG 400 is used in HP printers.
Hey!
I have question about this sort of banding.
I read that lower dryer temps or uni-direction will help me this one.
But this aroused another problem, the ink will not dry then! What should I do?
Haven't had the chance to try it out yet, but i'll give it a shot. I'm sure that if I'd have proper profile it would perform better. I use the MUTOH DSultra Semigloss 200g profile.
Maybe the ink dries on one side diffrently, because of the heater?
Our MUTOH is leaving white stripes* on the right side of the printer, but on the left evrything is ok.
*Stripes like when printing on high speed profile e.g. Banner 3
Nozzles check out. Don't know what else to check.