I want to thank all the members that have upgraded your accounts. I truly appreciate your support of the site monetarily. Supporting the site keeps this site up and running as a lot of work daily goes on behind the scenes.
Click to Support Signs101 ...
Fixed!
My colleagues and I found that if we heated the affected area with an electric heat gun from 2-4" away for about 2.5 mins the textured area flattened out. :rock-n-roll:
I've encountered an issue with 3M's 8518 laminate. Clear vinyl panels were labeled using pre-mask tape. When the tape was removed it left a textured mark on the laminate. I've tried applying heat to the surface with no avail. Any insight into possible fixes would be much appreciated. Thanks in...