• I want to thank all the members that have upgraded your accounts. I truly appreciate your support of the site monetarily. Supporting the site keeps this site up and running as a lot of work daily goes on behind the scenes. Click to Support Signs101 ...

Drytac SpotOn Clear tunneling on the 700W.

dypinc

New Member
I using the preset that is available online for 5 layer. At time it is fine and then I will get a section that starts to tunnel. Anybody have any advise for this problem.
 

Attachments

  • IMG_1768.JPG
    IMG_1768.JPG
    3.1 MB · Views: 119
  • IMG_1769.JPG
    IMG_1769.JPG
    3.5 MB · Views: 94

balstestrat

Problem Solver
How much curing heat on that profile? With 5L it's absolutely cooking in the oven for a while so you may want to go down and make sure drying is as high as it goes.
On another note, maybe some alternative media is a better match for that application.
 

dypinc

New Member
It appears the it was a defect in the roll as it only appeared in 2 places so far and it was before it got to the curing area.
 