• I want to thank all the members that have upgraded your accounts. I truly appreciate your support of the site monetarily. Supporting the site keeps this site up and running as a lot of work daily goes on behind the scenes. Click to Support Signs101 ...

Finishing HDU

abadsvt

New Member
Hi Guys, Not sure if this is the spot to post this in but I am building an HDU sign for a customer. I designed it then took it down to a wood working shop and had them CNC router it. It came out beautiful. So now since this is my first HDU sign i was curious on finishing it. I read tons of threads but noticed that I didn't see anything about home depot latex paint. The customer wants to pick out the colors and thought for convence on getting materials and colors that the new line of Baer primer paint would be a good choice but wanted to hear from the experts! I read that 1-shots primer is the best but wasn't sure if there was any other good primers that might be ready available at the depot. Home depot is just 1/4 mile from my shop. That is the reason for using them plus easy for the customers to be responsible for the color picking. Thanks and will take pics after the sign is all done!

Josh
 

abadsvt

New Member
Whenever I use HDU, I always lean toward good old house latex paint. Works wonderfully!
Thats what i thinking also. I just read about "SIGNPRIME" primer and sounds nice. It is pretty expensive though but being able to sand the primer sound like a good thing. You ever use house hold latex primers? Thanks
 

G-Artist

New Member
We get at least a 1/2 dozen sign and industry trade mags here and I have been reading about HDU since it came out. Never used it myself.

All, to a one, stated that it is best to use the recommended primer and use it as prescribed in the literature. Then you can use any paint you wish as a topcoat.
 

petrosgraphics

New Member
we use a lot of HDU, over the years....before you get started priming, make sure you
sand the surface with 220 grit sandpaper get rid of as many scratches,scrapes, etc.
as you can find... we use ben moore fresh start latex primer, found this to work real good.
i am sure any good latex primer would work, we have stuck with the fresh start for it works for us.... if you put 4 coats of primer sand each coat with 220 paper you should be ok... as for your finish coat, oil or latex does not really matter
 

Salmoneye

New Member
I like to use oil base for anything that I want to last. I would not use any paint from a box store like Home Depot. Even if it is the same brand as they sell in their professional paint stores it will almost certainly be a different formula with less solids etc... When I used to buy tons of Glidden, the cheapest paint in the pro store was better than the top of the line in the box store.
2 cents
 

JK driver

New Member
We use automotive primer and paints. We spray the panel with a good high fill automotive primer sand with a DA. Also make sure to prime the back to avoid warping. This is caused by primer/paint shrinking during the curing process. Priming the back will counteract this. Fill any pin holes left. Paint with a good gloss automotive paint. Then Gerber mask the panel rout it then prime and paint the copy. Peal the mask and it is done. This will last a long time!

The analogy I use is: How often do you paint your house? And how often do you paint your car???:beer
 

abadsvt

New Member
Thanks guys for the help and knowledge. I thought it might be benificial to see the size fo the products that i am doing. The small address sign is aprox 15" x 25" and the larger sign is a 24" x 36". Also i added a pic of whats getting painted on the larger side so you can invision what i am doing. If you look at the larger HDU sign i have going you'll notice that on the right side in the middle is a saw cut that isn't suposed to be there. What would you guys recommend on filling that saw cut? THanks again everyone!
 

Attachments

  • HDU before paint.jpg
    HDU before paint.jpg
    70.8 KB · Views: 432
  • HDU before painting.jpg
    HDU before painting.jpg
    75.6 KB · Views: 407
  • HDU art.jpg
    HDU art.jpg
    102.1 KB · Views: 385

k.a.s.

New Member
As was said, sand first try and get it as smooth as possible. We use Signprime, it works well and you can sand it smooth in between coats. It is pretty hard to get a nice smooth backround surface when you are hand painting around all those letters. I usally use a solid color stain on the backround, I like the contrast of that vs the high gloss on the letters. I finish with Ronan paints, we mix a color if we have to match somthing. One Shot has a lot of colors that you can use as well.

Kevin
 

Mosh

New Member
about home depot latex paint

That would be like restoring a classic car and then spray painting it with krylon.
Use a good paint and primer like Ronan, something made for a long life. That crap HD sells is for DIY people who don't know what they are doing anyway, so won't know a quality paint.
 

signmeup

New Member
That would be like restoring a classic car and then spray painting it with krylon.
Use a good paint and primer like Ronan, something made for a long life. That crap HD sells is for DIY people who don't know what they are doing anyway, so won't know a quality paint.
Baloney. I use Home Hardware 1080 latex primer. You don't have HH down there so go to a good paint shop and ask for something to prime plastic house siding that is sandable. Wash the sign with a garden hose before you prime it. Blowing it off with air won't get the dust out of the "pores".
I use a brush to prime the panel (2 coats) sand it between coats with 320 grit. (A roller won't get the paint into the "pores".) Then use foam rollers for the top coats, again latex house paint. Pittsburg Sunproof is good. It drys without tac which is real nice when you want to gild the lettering and not the whole sign. BTW....carving and painting through a mask will save you a ton of time....next time.
 
there are quite a few signmakers who DO NOT prime hdu at all...and before you say it, no they are not hacks. if you are using a low poundage then you will probably need to prime to fill the holes but the heavier stuff some people only prime to achieve light textures by crumpling a brush for small peaks and valleys or a rough roller for light bumps.

here is some technical data http://www.signfoam.com/tech.php?mode=finishing

myself i avoid high build primers like the plague invest in higher pound sheets and save yourself a tremendous amount of finishing labor.
 

abadsvt

New Member
there are quite a few signmakers who DO NOT prime hdu at all...and before you say it, no they are not hacks. if you are using a low poundage then you will probably need to prime to fill the holes but the heavier stuff some people only prime to achieve light textures by crumpling a brush for small peaks and valleys or a rough roller for light bumps.

here is some technical data http://www.signfoam.com/tech.php?mode=finishing

myself i avoid high build primers like the plague invest in higher pound sheets and save yourself a tremendous amount of finishing labor.


That is a good point. Both signs are 15lb foam. When you mention higher pound foam are you refering to 20lb and up? Thanks

Josh
 

abadsvt

New Member
That would be like restoring a classic car and then spray painting it with krylon.
Use a good paint and primer like Ronan, something made for a long life. That crap HD sells is for DIY people who don't know what they are doing anyway, so won't know a quality paint.


I am a classic car buff so thanks for putting it that into my language! :biggrin:

Josh
 

abadsvt

New Member
Baloney. I use Home Hardware 1080 latex primer. You don't have HH down there so go to a good paint shop and ask for something to prime plastic house siding that is sandable. Wash the sign with a garden hose before you prime it. Blowing it off with air won't get the dust out of the "pores".
I use a brush to prime the panel (2 coats) sand it between coats with 320 grit. (A roller won't get the paint into the "pores".) Then use foam rollers for the top coats, again latex house paint. Pittsburg Sunproof is good. It drys without tac which is real nice when you want to gild the lettering and not the whole sign. BTW....carving and painting through a mask will save you a ton of time....next time.


Thats a good idea. I will call the local paint store (not home depot). Thanks for the help!

Josh
 
yes higher density like 20# and i understand that it can be hard to obtain if you do not have a distributor that can justify stocking a large selection of sheet thicknesses and a variety of densities because they will usually default to the lower densities because they are cheaper per sheet.

there are a few brands out there as well signfoam, duna, etc. duna used to be very generous in providing a nice box of samples approx 1' X 2' in a variety of densities. i would highly recommend requesting them so that you can experiment without having to buy a sheet.
 

diverscott

New Member
Another thought on "justifying" going with the higher poundage:

"The money you save on materials, you'll spend on labor getting it right."

We use 20# and spray auto primer and paint (with hardener).
 

NY Signman

New Member
MOST IMPORTANT FIRST STEP..................... BLOW THE HDU OFF REALLY WELL! Run your hand over surface while using air gun.....bleed off any water in line prior also.

Can't tell you how many times over the 15yrs using, that while you peel off mask after gold leafing, something lifts back to the bare HDU. When you think it's blown off enough, go over it again. Haven't had a problem in over 5yrs.

Fresh Start, 2-3 coats, then into whatever finish you wish......I've brushed Chromatic, One-Shot, Latex, have also sprayed and rolled....all the mentioned.

The HDU of today...........soooooo much tighter cells and smoother then the orig. precision board we started with!

GREAT STUFF!!! Always recommend it to my customers for ANY high end sign....especially w/gold leaf.

Good luck
 

signmeup

New Member
I have found that blowing the dust off is not good enough. That dust sticks like it was designed to.

I recommend blasting it with a garden hose. The only thing I've seen about useing auto primer on HDU from a manufacturer was they didn't recommend it. Why? Who knows. It worked fine for me. I just don't like useing it. Latex primer for plastic house siding worked fine for me and the brand I use sands great.
 