Hello Guys,
We mainly do decorative window films (frosted, printed optically clear, contour cut, etc) and large wall installations. Have done some smaller anti graffiti film here and there, but now we have been asked to do an entire building, with many windows being 2.4m (8') high by2.1m (7') wide. So we will need to join the film on the window as they are both wider and longer than maximum roll width.
Having done lots of butt joins on wall vinyls, we though this should not be a problem. Did a trial in our studio window and we are not happy with the result. There is a 1/16" fine line where we cut the butt join. Please see photo attached showing the line on the glass and also the shadow of it on a sheet of paper behind the glass (sorry for messy writing, done on my phone). I can't make it disappear. I have left it to dry for a day and pressed it down again. I have tried to heat it gently with a heatgun, it does not go away.
It seems the me, that because of the thickness of the film, it does not lay completly flat once cut, so it's just a tiny bit too long for the space.
The film is 3M AG4.
Is there someone around who had experience with this? Could you please help? What would you do, how would you join the film?
Thanks so much
We mainly do decorative window films (frosted, printed optically clear, contour cut, etc) and large wall installations. Have done some smaller anti graffiti film here and there, but now we have been asked to do an entire building, with many windows being 2.4m (8') high by2.1m (7') wide. So we will need to join the film on the window as they are both wider and longer than maximum roll width.
Having done lots of butt joins on wall vinyls, we though this should not be a problem. Did a trial in our studio window and we are not happy with the result. There is a 1/16" fine line where we cut the butt join. Please see photo attached showing the line on the glass and also the shadow of it on a sheet of paper behind the glass (sorry for messy writing, done on my phone). I can't make it disappear. I have left it to dry for a day and pressed it down again. I have tried to heat it gently with a heatgun, it does not go away.
It seems the me, that because of the thickness of the film, it does not lay completly flat once cut, so it's just a tiny bit too long for the space.
The film is 3M AG4.
Is there someone around who had experience with this? Could you please help? What would you do, how would you join the film?