Graphics2u
New Member
First time I've Used FDC (probably the last). Only used it because I needed a matte finish with air release, this is what supplier had.
When printing on Mutoh 1614 it wrinkles along the edges. I've turned heat on Pree and Platen heaters way down to 35 degrees. And if anything theat made it worse.
Anyone used this before or have suggestions?
Thanks.
When printing on Mutoh 1614 it wrinkles along the edges. I've turned heat on Pree and Platen heaters way down to 35 degrees. And if anything theat made it worse.
Anyone used this before or have suggestions?
Thanks.