iSign, another great idea I wished I'd thought of doing.
Marlene, Yet another great idea. I guess we were just hung up on what the customer wanted which was for us to recreate the same thing he had.
MikePro, we waited three days for the latex before the clear coat. Then another day for that before application. It's just too dang humid here right now and like most of you I believe the outgassing is the major problem.
AUTO FX, I think the foil is holding the moisture now.
Techman, you are right about the compression problems on the "E". I was dead tired when I applied that "E" and made it a point to start at the vertical stroke so each horizontal stroke could fall as it wanted. But then, as tired as I was and working so late, I started application at the end of the horizontal strokes toward the vertical. I was cussing myself as I got half-way through it almost knowing that it was going to become an issue.
joeshaul, enlightening information on FDC. I knew none of that. I have had very little experience with foils. What I did have caused me to stay away from it as much as I could. We've only used it a few times on some truck stuff and that worked out ok but a pain regardless.
Steve, good information too.
This sign should be done tomorrow. I'll post a pic unless it's embarrassing. lol