shadi75
owner
HI
I had somthing happend with a customer that i never seen before.
This customer bought a 5ft long decal from me, it was made with the orajet 3551 RA and laminated with the 290g, i also placed the installation masking tap so it very easy to install.
now he claims that during the installation he peeled off one side to removed some bubble and some of the clear coat came off.
My first question was how long you had the clear coat on, he said over 5 years, he as a 64 chevy show carthat he did a very expensive paint job on 5 years ago.
Now i talked to oracal and they told me that his clear coat was proabably getting poor and that now way the adhesive would of did that .
The other thing i want add is that the decal was made about 6 month ago and it was sitting in my office in room temperature all of this time.
Let me know what you guys think.
Thanks
I had somthing happend with a customer that i never seen before.
This customer bought a 5ft long decal from me, it was made with the orajet 3551 RA and laminated with the 290g, i also placed the installation masking tap so it very easy to install.
now he claims that during the installation he peeled off one side to removed some bubble and some of the clear coat came off.
My first question was how long you had the clear coat on, he said over 5 years, he as a 64 chevy show carthat he did a very expensive paint job on 5 years ago.
Now i talked to oracal and they told me that his clear coat was proabably getting poor and that now way the adhesive would of did that .
The other thing i want add is that the decal was made about 6 month ago and it was sitting in my office in room temperature all of this time.
Let me know what you guys think.
Thanks